UNS N08811 Seamless Pipe
video

UNS N08811 Seamless Pipe

UNS N08811 seamless pipe is an ideal material choice for applications requiring strong corrosion resistance in reducing environments and high-temperature performance. Its unique combination of materials provides superior performance in extreme environments compared to traditional stainless steels and nickel-based alloys.
Отправить запрос
Теперь говорите

Являясь ведущим поставщиком и производителем в Китае, компания GNEE Steel предлагает экономичную-эффективную- продукцию из сплавов на основе никеля.

Внедрение продукции

 

Super alloys are also referred to as high performance alloys. They have good creep and oxidation resistance, and are utilized where high surface stability is required. They also have an ability to function under high temperatures and mechanical stress. They can be strengthened by solid-solution hardening, work hardening, and precipitation hardening. They are divided into three groups such as iron-based, nickel-based, and cobalt-based alloys.

560 MPa 81200 psi
250 MPa 36300 psi
45% 45%

The thermal properties of Incoloy 800HT™ are given in the following table.

Thermal expansion co-efficient (@ 20-100 degree /68-212 degree F) 14.4 µm/m degree 8.00 µin/in degree F
11.5 W/mK 79.8 BTU in/hr. ft². degree F

UNS N08811 seamless pipeUNS N08811 seamless pipeUNS N08811 seamless pipe

 